Guides / Choosing a Supplier
Cosmetic Defect Definitions for Machined Audio Parts: From Dents to Pits
November 10, 2026

A cosmetic defect is any visible flaw on a face that the buyer will see, and the same flaw gets a different name in different shops. A shop that calls a mark a “scratch” and a brand that calls it a “gouge” are arguing about the price of a remake. This glossary defines the common terms, shows where each one comes from in machining and anodizing, and finishes with a checklist you can paste into a drawing note.
One caution first. No public standard gives one set of limits for every part. ISO 8785:1998 is the international vocabulary for surface imperfections, but by its own scope it does not say which imperfections are acceptable, because that depends on the part’s function. The definitions below come from one published supplier cosmetic standard (Viasat PR001336, rev 002) and from machining and anodizing references. Treat them as a starting vocabulary, then agree your own limits with the shop.
Marks from the machining stage
| Term | Definition | Where it comes from |
|---|---|---|
| Scratch | A shallow groove that can be seen but not felt | Handling, chips dragged across a face, loose parts in a tray |
| Scuff or abrasion | Very light scratches, or a surface change with no material removed | Parts rubbing in a bag or a tray |
| Gouge | A groove that extends through the finish into the metal, with a measurable depth | A sharp object, a dropped tool, a chip caught in the fixture |
| Nick | Like a gouge but short, caused by an impact | Knocks on edges |
| Dent | A surface depression caused by an impact | Dropped parts, parts hitting each other |
| Ding | A roughly funnel-shaped dent | A point impact |
| Burr | A raised edge or small piece of material left after machining | Milling, drilling, turning, engraving |
| Pit | Small craters on the surface | Corrosion, chloride in the bath or pretreatment |
| Tool mark | The pattern the cutter leaves on the surface | Normal process, becomes a defect when uneven or too deep |
| Chatter | Regular waves on the surface from vibration | Tool or workpiece vibration during the cut |
Two details are worth knowing.
Burrs come in types. Wikipedia names three types: the rollover burr, where the edge bends over (the most common), the Poisson burr, where material flows sideways and the breakout burr, where material tears away. Hand deburring is itself a common way to add scratches to a visible edge, so a defined chamfer on a visible face is a better answer than “deburr all edges”, see diamond cut chamfers on audio panels.

Chatter is a process signal, not just a mark. Wikipedia’s article on machining vibrations describes chatter as marks left by vibration, from forced vibration such as interrupted cutting and runout, or from vibration that builds up as the cutter follows its own earlier pass. A long tool with a high length-to-diameter ratio and low holder stiffness is a common source. Because the cause is in the setup, chatter tends to repeat from part to part rather than appear on one piece.
Marks from the finishing stage
| Term | Definition | Where it comes from |
|---|---|---|
| Rack mark | Where the part touched the conductive rack, with the coating missing or thinner | Anodizing, electrical contact is needed |
| Burn | Dark, powdery or rough patches, often at edges or contact points | Too much current in one spot, poor contact |
| Chloride pitting | Pits with no anodic film over them | Contaminated bath or pretreatment |
| Streaking | Bands of different brightness along the part | Metal structure in extruded stock |
| Staining | Marks left on the surface | Residual oil, oxide or smut from poor cleaning |
| Oxide bloom | A powdery white residue or smudge | A poor seal or contaminated seal |
| Soft or dusty coating | A coating that feels dusty or soft | Bath chemistry out of balance |
| Discoloration | Any change from the original colour or shade | Dye, alloy, thickness or lot differences |
| Fingerprint | An impression left by handling | Bare hands on bare or finished metal |
The rack mark gets the most disputes, because it cannot be avoided. Fictiv explains that anodizing is electrochemical and every part needs electrical contact with the rack, so a mark is unavoidable somewhere. The fix is placement. MIL-PRF-8625 section 3.13.1 asks that the number and size of contact marks are kept to a minimum, and the location is as specified on the drawing. Put the rack point on a hidden hole or an inner face. See threads in anodized chassis for the related masking questions.
Streaking has a different cause. The aluminium-guide site describes streaks as differences in brightness caused by a non-uniform metal structure at the surface, from billet structure, extrusion settings or die design. Because the oxide film is transparent, the finished look mostly reflects the metal underneath, so a streak in the metal shows through the coating. If you machine from extrusion, one source suggests asking for one extruder and one lot of metal, and see billet, extrusion or sheet.
ASTM B580-25 gives the baseline for the coating as a whole: each anodic coating should be continuous, smooth, adherent, uniform in appearance and free of powdery areas. That is why a powdery patch or an uncoated area is normally treated as a coating defect, while a rack mark needs a drawing note on where it may sit.
Why a name alone does not settle a dispute
A definition says what the mark is. It does not say whether the part passes. Two things decide that.
- The surface class. The Viasat standard splits surfaces into class A (a critical surface usually seen close up by the user, such as a front panel), class B (an exterior surface next to class A, easily seen) and class C (rarely viewed or internal). The same dent can be a reject on class A and a pass on class C.
- The viewing conditions. The same standard inspects class A from 24 inches (610 mm) and class B from 30 inches (760 mm), allows 5 seconds per 50 square inches on a front panel, uses uniform light of 750 to 1250 lux, and does not allow magnification for judging a cosmetic defect. These are one company’s numbers, not an industry norm, but they show what a complete rule contains. Our guide to cosmetic inspection lighting and viewing distance covers how to set your own.
Need a quote for this part? Get a quote for your audio parts
A checklist to write into the drawing
- Name the faces. Mark class A, B and C faces, see specifying cosmetic faces on a machining drawing.
- Choose the defect words from one list. Use the table above or your own, and attach it to the PO so both sides read the same one.
- Set a rule per class. For example: class A, no gouge, nick, dent, pit or burr; scratches only if they cannot be felt and are not seen at the agreed distance and time. Adapt it, do not copy it.
- State the rack point. Name the hidden feature where contact marks are allowed.
- Say what the cutter may leave. Define whether tool marks are allowed on class A, and what Ra the face should reach, see surface roughness on cosmetic faces.
- Fix the viewing conditions. Distance, time, light level, and no magnification.
- Agree a limit sample. A physical part at the edge of acceptable settles what words cannot, see first article inspection for cosmetic parts.
- Cover the packing. A part that passes at the shop can fail in transit, see packing finished audio parts.
A cosmetic finish can also be chosen to hide the marks you cannot avoid. A bead blast or a vibratory finish evens out fine tool marks and light scratches, see bead blasting audio enclosures and vibratory finishing for small audio hardware. It does not hide a gouge or a dent.
Using the glossary in an RFQ
Attach the glossary or your own version to the drawing, mark the class A faces and add the viewing conditions. Shops quote a cosmetic job more accurately when the rule is written, and the quotes are easier to compare. If you are choosing between shops, see how to choose the right machine shop for audio parts. Send the drawing through the RFQ form and we reply within 24 business hours with one itemised quote for the finished parts. Work goes to partner shops that make cosmetic audio parts.
Sources
- Viasat Cosmetic Inspection Criteria PR001336 rev 002 (one supplier’s published standard, used for definitions and viewing conditions)
- ISO 8785:1998 listing, Geometrical product specification, surface imperfections
- Burr (edge), Wikipedia
- Machining vibrations, Wikipedia
- What are rack marks in anodizing, Fictiv (vendor content, directional)
- Anodized aerospace defects, Valence Surface Technologies (vendor content, directional)
- Streaking defects in anodised aluminium, aluminium-guide
- Anodized finishes: avoiding color variation, The Construction Specifier (author works for a finisher, directional)
- ASTM B580-25 Standard Specification for Anodic Oxide Coatings on Aluminum
See also: cosmetic surface classes A, B and C and how to assign them.
Frequently asked questions
What is the difference between a scratch and a gouge?
One published supplier standard defines a scratch as a shallow groove that can be seen but not felt. A gouge is a groove that goes through the finish into the metal and has a measurable depth. On an anodized panel a gouge shows bare or damaged metal under the coating, so it is usually a reject where a faint scratch may not be.
Are tool marks a cosmetic defect?
Not by default. A cutter always leaves a pattern, and it is the reason the finish is specified. They become a defect when they are deeper than the finish can hide, change from one area to another, or show chatter. Say on the drawing which faces must have no visible tool marks and what finish hides them.
Is there an ISO standard that defines surface defects?
ISO 8785:1998 defines terms and parameters for surface imperfections, separate from roughness and waviness. It gives a shared vocabulary but does not say which imperfections are acceptable, because that depends on the application. The full text is sold by national standards bodies, so most buyers write their own limits.
What is a rack mark on an anodized part?
A rack mark is the spot where the part touched the conductive rack during anodizing. The coating is missing or thinner there because the part needs electrical contact. MIL-PRF-8625 asks that the number and size of contact marks are kept to a minimum and placed where the drawing specifies.
Need a quote for this part?
Send the drawing. We quote the finished parts, place the work with a partner shop and reply within 24 business hours.
Get a quote for your audio parts